Dab tsi yog iav-melting electrode?
Cov iav melting electrode yog siv nyob rau hauv lub khob rauv los ua cov iav zoo thiab iav fiber ntau.
Cov khoom siv iav melting electrode
Lub iav melting electrode yuav tsum muaj peev xwm tiv taus qhov kub thiab txias heev thiab hnyav iav melting. Raws li cov yam ntxwv ntawm cov khoom,molybdenumyog cov khoom tsim nyog tshaj plaws kom ua tau raws li cov xwm txheej nyuaj no:
1. Melting point 2620 degree C
2. High purity
3. Zoo heev los tiv thaiv creep
4. Dimensional stability
5. Zoo heev corrosion kuj
6. Zoo conductivity thiab thermal conductivity

Kev siv cov molybdenum electrodes hauv iav kev lag luam
1. khob dej, ntim khoom noj, thiab cov tais diav;
2. Cov iav qhov rais ntawm tsev, chaw ua haujlwm, thiab tsheb;
3. Lub vaj huam sib luag ntawm cov khoom siv hluav taws xob thiab lub hnub ci;
4. Ntau lub thawv ntim khoom lag luam thiab kev tshawb fawb.