Biomedical titanium alloy: Classification, Performance

Jun 21, 2022

Biomedical titanium alloys tuaj yeem raug cais raws li cov qauv ntawm cov khoom siv. Hom, ntxiv rau Hom, thiab Titanium alloy hom III. Tam sim no, ntshiab titanium thiab Ti-6Al-4V alloy tseem siv dav hauv kev kho mob. tab sis Titanium-hom alloys tau dhau los ua cov ntsiab lus kev tshawb fawb kub hauv daim teb no vim lawv qhov qis elastic modulus thiab zoo biocompatibility. Nws yog qhov zoo tshaj plaws biomedical titanium alloy.

titanium rods the medical metal of choice

Table 1 qhia cov khoom siv kho tshuab ntawm ntau yam biomedical titanium alloys. Daim duab 1 qhia txog kev sib piv ntawm elastic modulus ntawm ntau yam biomedical alloys nrog cov pob txha ntawm tib neeg. Raws li koj tau pom, Lub elastic modulus ntawm lub thib ob tiam biomedical titanium yog ho qis dua li ntawm thawj tiam. Muaj kev nce ntxiv hauv Nb cov ntsiab lus hauv kev tsim alloy thiab ob qho tib si yog Titanium alloy hom, Ti-35Nb-7Zr-5Ta thiab Ti-29Nb-13 Ta-7.1Zr alloys muaj qhov qis tshaj elastic modulus ntawm 55MPa, uas yog qhov ze tshaj plaws ntawm tib neeg cov pob txha. Yog li ntawd, txoj kev loj hlob ntawm biomedical cov ntaub ntawv uas tsis tshua muaj elastic modulus Ti-type alloy tau dhau los ua kev tshawb fawb hotspot nyob rau hauv daim teb no. Biomedical hyperelasticity, feem ntau tau kawm nyob rau hauv tsev thiab txawv teb chaws Titanium alloy yog ti NB hyperelastic Titanium alloy.

Table 1 Mechanical Properties of biomedical titanium


Khoom siv

Txuj

Elastic Modulus/Gpa

Tensile zog / Mpa

Hom alloy

Thawj tiam biomaterials


Kev lag luam Pure Titanium

ASTM 1341 (SIB 1341)

100

240-550

a

Ti-6Al-4V Forged thiab dov daim

ASTM F136

110

860-965

ib plus

Ti-6Al-4V

Standard Level

TIAB SA 1472

112

895-930

ib plus

Ti-6AI-7Nb

ASTM F 1295 Cov Lus Qhia

110

900-1050

ib plus

Ti-5Al-2.5Fe

110

1020

ib plus

Thib ob thiab thib peb tiam biomaterials


Ti-13Nb-13Zr

79-84

973-1037

Metastable

Ti-12Mo-6Zr-2Fe

74-85

1060-1100

Ti-35Nb-7Zr-5Ta

55

596

Ti-29Nb-13Ta-4.6Zr

65

911

Ti-35Nb-7Zr-5Ta-0.4o

TIAB SA 1713

66

1010

Ti-15Mo-5Zr-3AI

TIAB SA 1813

82

Ti-Mo

ASTM F 2066 Cov Lus Qhia

Comparison of elastic modulus between biomedical alloy and human bone