Raws li cov khoom siv electrode, platinum muaj cov yam ntxwv ntawm kev tiv thaiv corrosion, siab electrocatalytic kev ua haujlwm, siab oxygen evolution peev xwm, thiab tsis tshua muaj hydrogen evolution peev xwm. Txawm li cas los xij, nws qhov tsis txaus thiab tus nqi siab txwv rau daim ntawv thovplatinum{0}}coated titanium anodehauv kev lag luam electrochemical. Lub platinum-titanium anode yog ib qho tshwj xeeb electrode uas muaj zog tshwj xeeb, thermal stability, muaj zog corrosion{1}}kuj, thiab zoo heev tus kheej-passivation muaj peev xwm. Lub anode npaj los ntawm cov txheej txheem tshwj xeeb muaj kev ua tau zoo ntawm cov ntshiab platinum electrodes, uas tuaj yeem txo cov nqi zoo heev. Yog li ntawd, nws tau dav siv nyob rau hauv electrochemical teb.
Kev npaj technology ntawmplatinum{0}}coated titanium anode
Tam sim no, txoj kev npaj ntau ntawm platinum{0}}titanium anode yog lub cev vapor deposition, electroplating, thiab sintering.
1. Lub cev vapor deposition:
Cov txheej yog npaj los ntawm lub tshuab nqus tsev ion plating thiab magnetron sputtering. Cov txheej txheej npaj los ntawm txoj kev no muaj lub zog sib txuas nrog cov matrix thiab cov thickness tswj tau, tab sis nws yog npaj rau hauv lub tshuab nqus tsev chamber, yog li nws yog ib qho nyuaj rau kev npaj cov txheej rau cov cheeb tsam loj thiab cov duab complex workpieces vim muaj kev txwv ntawm cov khoom siv.

2. Electroplating:
Txoj kev siv tam sim no los txo cov hlau ions hauv cov tshuaj electroplating rau platinum hlau ntawm cathode (workpiece), suav nrog molten ntsev electroplating thiab dej tov electroplating. Molten ntsev electroplating tsis tshua siv vim nws cov txheej txheem nyuaj, ib puag ncig kev ua haujlwm tsis zoo, thiab tus nqi siab. Aqueous kua electroplating muaj qhov tsis zoo ntawm cov txheej txheem electroplating nruj thiab teeb meem txij nkawm ntawm cov tshuaj electroplating. Tam sim no, nws tsuas yog siv rau hauv cov khoom siv kho kom zoo nkauj thiab kev tiv thaiv cov txheej txheem xws li kho kom zoo nkauj, cutlery, khoom siv kho mob, cov cuab yeej tshawb fawb, thiab lwm yam.
3. Sintering txoj kev:
Cov txheej txheem yog npaj los ntawm txhuam thiab siab -kub sintering, uas yog yooj yim nyob rau hauv tus txheej txheem, tsis tshua muaj nyob rau hauv cov khoom yuav tsum tau, uas muaj peev xwm tsim loj cheeb tsam thiab complex workpieces. Cov txheej muaj adhesion zoo thiab uniformity, zoo heev electrochemical kev ua tau zoo, thiab kev pab lub neej, nws yuav siv tau rau ntau lub hom phiaj.
Yog tias koj tab tom nrhiav rau tus neeg muag khoom ntawmplatinum{0}}coated titanium anode, thov hu rau peb ntawmfairytitanium@gmail.com.