Cov qauv kev lag luam tseem ceeb rau Titanium Bars: Ua kom zoo thiab ua tau raws li qhov ua tau zoo

May 09, 2023

Muaj ntau cov qauv kev lag luam uas siv rau titanium tuav. Qee qhov feem ntau muaj xws li:

1. ASTM B348 - Standard Specification rauTitanium thiab Titanium Alloy Barsthiab Billets: Qhov kev qhia tshwj xeeb no suav nrog cov titanium thiab titanium alloy tuav thiab billets hauv qib sib txawv.

2. ASTM F67 - Standard Specification rau Unalloyed Titanium, rau kev phais phais (UNS R50250, UNS R50400, UNS R50550, UNS R50700): Qhov kev qhia tshwj xeeb no suav nrog cov tshuaj lom neeg, khoom siv, thiab cov khoom siv hlau rau cov khoom siv titanium thiab cov khoom siv tsis siv neeg. siv nyob rau hauv phais implants.

3. ASTM F136 - Standard Specification rau Wrought Titanium-6Aluminum-4Vanadium ELI (Ntxiv Qes Interstitial) Alloy rau Kev Kho Mob Kev Kho Mob (UNS R56401): Cov lus qhia tshwj xeeb no suav nrog tshuaj lom neeg, tshuab, thiab metallurgical xav tau rau wrought titanium-6aluminium-4vanadium ELI tuav thiab billets siv nyob rau hauv kev phais implants.

4. AMS 4928 - Titanium Alloy Bars, Hlau, Forgings, Rings, thiab Drawn Shapes 6Al - 4V, Annealed: Qhov kev qhia tshwj xeeb no npog cov titanium alloy hauv daim ntawv tuav, hlau, forgings, rings, thiab kos duab.

5.2-2 - Kev cog qoob loo rau kev phais - Cov khoom siv hlau - Ntu 2: Cov titanium tsis siv neeg: Cov qauv no qhia txog cov yam ntxwv ntawm, thiab cov qauv kev sim sib xws rau, tsis muaj titanium rau kev siv hauv kev tsim cov khoom siv phais.

6. ISO 5832-3 - Kev cog qoob loo rau kev phais - Cov khoom siv hlau - Ntu 3: Wrought titanium 6-aluminium 4-vanadium alloy: Cov qauv no qhia txog cov yam ntxwv ntawm, thiab cov qauv kev sim rau, wrought titanium { {5}}aluminium 4-vanadium alloy siv rau hauv kev tsim cov khoom siv phais.

Cov qauv no xyuas kom meej tias titanium tuav tau raws li cov kev cai tshwj xeeb, kev siv tshuab, thiab metallurgical thiab tsim nyog rau lawv daim ntawv thov.