Titanium alloy yog lub npe hu ua cov hlau niaj hnub. Vim tias nws tau siv dav hauv kev tshawb fawb txog kev tiv thaiv hauv tebchaws thiab thev naus laus zis, Tebchaws Asmeskas thiab lwm lub zog tub rog muab qhov tseem ceeb rau nws txoj kev loj hlob thiab kev siv, qee cov kws tshawb fawb txuas ntxiv mus kawm cov hlau. Kev tshawb fawb ntawmsiab - kub titanium alloyyog active txawv teb chaws. vim yog siv nyob rau hauv aircraft engine compressor disc, lub cav yuav tsum siab - kub cov ntaub ntawv kom muaj zoo chav tsev kub kev kawm thiab thermal stability, uas muaj contradictory yuav tsum tau rau cov khoom muaj pes tsawg leeg thiab cov qauv.
Tom qab xyoo 1950, qhov kev pabcuam kub ntawm titanium maj mam nce, daim ntawv thov kub ntawmsiab - kub titanium alloymus txog 600 degree thaum pib ntawm lub xyoo pua 21st.
Tam sim no, tshiabsiab - kub titanium alloysntse siv nyob rau hauv cov tub rog thiab civil aircraft xyaw xws li IMI834 los ntawm teb chaws Aas Kiv. High - kub alloys xws li Ti55, Ti53311S thiab Ti60 tau tsim nyob rau hauv Suav teb. Tam sim no, nws txoj kev loj hlob hauv Suav teb tsis tau ua tiav daim ntawv thov zoo hauv aviation. Tam sim no, tus nqi ntawm titanium siv hauv Aeroengine tau dhau los ua qhov ntsuas tseem ceeb los ntsuas nws qhov kev nce qib. Piv txwv li, lub thib plaub - tiam fighter F - 22 yog txawm peem rau nrog ib tug F119 engine, uas nws cov nqi ntawm titanium siv yog mus txog 35 %. High - kub titanium alloy yog siv los tsim cov khoom sib txuam ntawm cov tshuab aero. Tam sim no, titanium engineering nrog qhov kub siab tshaj plaws hauv ntiaj teb yog MI934.