Kev ntsuas kev tiv thaiv rau cavitation corrosion ntawm Ti-6Al-4V alloy - kev kho cua sov

Dec 01, 2021

Titanium alloymuaj tsawg hardness thiab tsis zoo hnav tsis kam. Thaum siv los ua cov khoom ntws ntws xws li lub nkoj propeller hniav, turbine hniav, turbines, cua ntsawj ntshab, twj, thiab li qub, nws yooj yim heev los ua cavitation ntawm cov khoom vim lub siab hloov chaw hauv cov kua. Thaum cavitation npuas vau nyob ze ntawm cov ciam teb ruaj khov, qhov chaw ntawm cov khoom siv yuav tev tawm, ua rau txo qis ntawm cov khoom siv, kev ua haujlwm luv luv, thiab txawm tias tsis ua haujlwm.titanium alloy cov khoom.

Cov txiaj ntsig tau pom tias cov cavitation tsis kam ntawmtitanium alloytuaj yeem txhim kho los ntawm kev hloov cov microstructure ntawm titanium alloy. Li Haibin kub khoTi-6Al-4V alloyntawm qhov sib txawv ntawm qhov kub thiab txias (1020 ℃, 950 ℃, thiab 850 ℃) kom tau txais cov qauv widmanstatten, qauv bimodal, thiab equiaxed qauv feem. Tom qab qhov kev sim 8 h cavitation hauv dej deionized, nws tau pom tias qhov poob phaus ntawm tag nrho cov qauv tau txais los ntawm kev kho cua sov tsawg dua li ntawm Ti-6A-l4V qub.

Ntawm lawv, cov qauv Widmanstatten tau txais los ntawm 1020 ℃ + dej quenching muaj qhov tsawg tshaj plaws cavitation qhov hnyav poob (77.9% ntawm cov qauv qub), thiab lub siab tshaj plaws cavitation corrosion coefficient (1.83 npaug ntawm cov qauv qub).

Txoj kev tshawb no qhia tau hais tias kuj muaj qee qhov sib txawv ntawm cov cavitation corrosion kuj ntawmTi-6Al-4V alloysnrog sib txawv microstructures. Widmanstatten qauv muaj martensite α ′ theem los yog lamellar α theem, uas txhim khu cov pob txha toughness thiab tensile lub zog ntawm Ti-6Al-4V, thiab cov khoom muaj peev xwm nqus tau lub zog li ntawm cavitation vau; Thawj theem α nyob rau hauv ob-lub xeev cov qauv muaj lub zog ua hauj lwm hardening muaj peev xwm, thiab lub β transformation qauv (thib ob α theem) yuav ua rau kom lub zog thiab hardness ntawm cov khoom, thiab nws kuj txhawb lub zog uas.Ti-6Al-4Vtuaj yeem nqus tau qhov tawg ntawm kab noj hniav; Txawm hais tias tus qauv equiaxed kuj muaj theem nrab α theem, nws cov ntsiab lus tsawg dua, yog li kev txhim kho ntawm kev ua haujlwm ntawm kev tiv thaiv kev ua haujlwm tsis zoo yog tsis pom tseeb li ntawm ob lub xeev cov qauv. Hauv qhov kev sim no, cov qauv Widmanstatten muaj qhov zoo tshaj plaws cavitation corrosion kuj, ua raws li ob lub xeev cov qauv, thiab cov qauv equiaxed muaj qhov qis tshaj cavitation corrosion kuj.