Titanium thiab titanium alloy qauv hauv ASTM
Titanium alloys raug cais raws li ntau yam qauv. Hauv Brazil, tus qauv siv dav tshaj plaws yog ASTM. Raws li tus qauv no, cov ntaub ntawv titanium ua raws li kev faib tawm hauv qab no:
B 265 - Phaj, ntawv, thiab strips rau titanium thiab titanium alloys hauv qib 1 txog 38
B299 - titanium daim txhuam cev
B 338 - nrog lossis seamless raj rau titanium thiab titanium alloys hauv qib 1 txog 38
B 348 - tuav thiab billets ntawm titanium thiab titanium alloys hauv qib 1 txog 38
B 363 - nrog lossis tsis muaj kev sib txuas vuam ntawm titanium thiab titanium alloys
B 367 - Cast titanium lossis titanium alloys
B 381 - Forged titanium lossis titanium alloys hauv qib 1 txog 38
F 67 - ntshiab titanium rau kev phais implants
F 136 - Titanium 6Al-4V alloy rau kev phais phais
F 467 - Txiv ntseej Titanium
F 468 - ntswj thiab titanium rooj plaub
F 1472 - Titanium alloy 6Al-4V forged rau kev cog hniav
Hauv Tebchaws Meskas, ntxiv rau lwm cov qauv ASTM tau siv, ntxiv dag zog rau cov titanium alloy:
• MIL (tub rog)
• DOD (Department. Of Defense)
• AMS (Specifications. Aerospace Materials)
• AIA (Association of Aerospace Industries)
• SAE (Society of Automotive Engineers)
• UNS (Unified Numbering System)
• ANSI (American National Standards Institute)
• ASME (American Society of Mechanical Engineers)
• AWS (American Welding Society)
Ntau lub teb chaws muaj lawv tus qauv, xws li lub teb chaws Yelemees nrog DIN, Fabkis nrog AFNOR tus qauv, Nyiv nrog JIS, Kauslim nrog KSA tus qauv, Tuam Tshoj nrog tus qauv CNS, UK nrog BSI tus qauv, thiab Russia nrog GOST / VT tus qauv. Nws tsis yog ib txwm muaj peev xwm nrhiav tau qhov sib npaug ntawm cov qauv.