TIG vuam nrog cerium tungsten electrode yog yuav tsum tau rautitanium phajthiabtitanium cevntawm titanium welded nkoj, nws zawj nto yuav tsum tsis muaj kab nrib pleb, delamination, inclusions, thiab lwm yam tsis xws luag.
Thaum lub tungsten electrode kov lub vuam hlau thaum vuam, lub vuam yuav tsum tau nres tam sim kom tshem tawm cov pa phem. Yog tias tsim nyog, qhov ntxeev ntawm tungsten electrode tuaj yeem polished ua ntej vuam. Titanium tsis zoo thermal conductivity thiab nws melting point yog 1668 degree, siab tshaj hlau thiab ntau lwm yam hlau, hlau intermediate tebchaw yog tsim nyob rau hauv lub molten lub xeev, uas ua rau embrittlement ntawm welded pob qij txha, Yog li ntawd, titanium thiab hlau tsis tuaj yeem fusion welded. Nws yog nruj me ntsis txwv tsis pub sib tov steel thiab lwm yam hlau nyob rau hauv tus txheej txheem ntawm titanium fusion vuam.

Nyob rau tib lub sijhawm, titanium muaj zog txo qis nyob rau hauv qhov kub-kub melting thiab tuaj yeem hnov mob nrog ntau yam ntsiab lus thiab cov tebchaw. Yog li ntawd, thaum weldingtitanium phaj thiab titanium yeeb nkab, pem hauv ntej ntawm tag nrho cov welds thiab sab nraum qab ntawm ib tug seam yuav tsum tau tiv thaiv los ntawm inert gas.
Cov neeg ua haujlwm vuam yuav tsum ua tau raws li qhov yuav tsum tau ua ntawm tungsten gas shielded vuam ntawm aluminium thiab aluminium alloy lossis titanium thiab titanium alloy. Lub vuam ib puag ncig muaj kev cuam tshuam zoo rau kev vuam zoo thiab kev sib koom ua haujlwm. Lub vuam yuav tsum tau ua nyob rau hauv ib puag ncig tsis muaj pa luam yeeb thiab tsis muaj plua plav. Yog tias cov cuab yeej siv steel siv nyob rau hauv tib lub rooj cob qhia, kev ntsuas kev sib cais yuav tsum tau ua kom ntseeg tau tiastitanium phaj thiab titanium yeeb nkabtsis muaj kuab paug los ntawm hlau thaum vuam.
Yog koj xav yuavtitanium daim hlau los yog cov kav dejrau cov hlab ntsha siab, thov hu rau peb ntawmtina@tmsalloy.com.