Dab tsi yog qhov txawv thiab nta ntawm titanium alloy TI -6242 VS TI -64?

Apr 18, 2023

Ob leeg titanium alloys TI -6242 thiabTSI -64yog alpha-beta titanium alloys thiab muaj cov tshuaj zoo sib xws. Txawm li cas los xij, muaj qee qhov sib txawv ntawm ob lub alloys:

1. Lub zog: TI-6242 muaj lub zog siab thiab tensile zog piv rau TI-64.

2. Ductility: TI-64 ductile ntau dua TI-6242.

3. Weldability: TI-64 yog weldable ntau dua TI-6242.

4. Corrosion kuj: TI-6242 muaj corrosion kuj zoo dua TI-64.

5. Nqe: TI-6242 kim dua TI-64.

Titanium alloy TI-6242V thiab TI-64 muaj cov yam ntxwv hauv qab no:

1. Lub zog siab: Ob leeg alloys muaj lub zog-rau-hnyav piv, cia lawv tiv taus kev ntxhov siab thiab thauj khoom yam tsis muaj deforming lossis tawg.

2. Kev tiv thaiv corrosion zoo heev: Cov alloys no muaj kev tiv thaiv corrosion hauv ntau qhov chaw, ua rau lawv zoo tagnrho rau kev siv hnyav.

3. Kev qaug zog ua haujlwm zoo: Ob leeg alloys muaj zog ua haujlwm zoo heev, ua rau lawv muaj peev xwm tiv taus ntau dua thiab kev ntxhov siab yam tsis ua haujlwm.

4. Kev ua haujlwm siab kub: Cov alloys no muaj cov cua sov zoo, ua rau lawv tuaj yeem tiv taus qhov kub thiab txias yam tsis muaj qhov poob ntawm lub zog lossis hardening.

5. Weldability: Ob lub alloys tau yooj yim weldable thiab tuaj yeem koom nrog ntau txoj kev xws li TIG, MIG, thiab laser vuam.

6. Tsawg ntom ntom: ob qho tib si alloys muaj tsawg ntom ntom, ua rau lawv lub teeb ci thiab ua rau lawv siv qhov hnyav-txuag yog qhov tseem ceeb.

7. Kev tsim khoom yooj yim: Ob leeg alloys yog ib qho yooj yim rau kev tsim thiab txheej txheem, tso cai rau kev tsim cov khoom tsim cov khoom siv nrog siab precision thiab sib xws.