titanium rebarstuaj nyob rau hauv ntau qib, txhua tus muaj cov khoom sib txawv kom haum rau ntau yam kev siv. Nov yog qee qib ntawm titanium rec bars thiab lawv cov khoom:
Qib 1: Kuj tseem hu ua kev lag luam ntshiab titanium, Qib 1 muaj 99.5 feem pua titanium ntshiab. Vim nws siab purity, nws muaj zoo heev corrosion kuj, formability, thiab weldability. Qib no yog qhov zoo tagnrho rau cov ntawv thov uas xav tau kev tiv thaiv corrosion siab, xws li kev ua tshuaj lom neeg, marine, thiab aerospace industries.
Qib 2: me ntsis muaj zog dua qib 1, Qib 2 tswj kev tiv thaiv corrosion zoo heev thiab zoo dua me ntsis ntawm cov khoom siv dag zog. Qib no yog qhov zoo tshaj plaws rau cov ntawv thov uas yuav tsum muaj zog dua tab sis weldability thiab ductility tseem tseem ceeb, xws li cov khoom siv hluav taws xob, cov hlab ntsha siab, thiab cov kav dej.
Qib 3: Qib 3 muaj zog dua qib 2 thiab muaj kev sib piv corrosion kuj. Txawm li cas los, nws yog tsawg formable thiab weldable. Nws yog qhov tsim nyog rau cov ntawv thov uas xav tau lub zog nruab nrab thiab zoo corrosion kuj, xws li cov khoom siv thiab cov khoom siv tsheb.
Qib 4: Qib 4 yog qhov muaj zog tshaj plaws ntawm cov khoom lag luam ntshiab titanium qib. Nws muaj kev tiv thaiv corrosion siab, tab sis nws cov formability thiab weldability tsis zoo li Qib 1 thiab 2. Cov qib no yog qhov zoo tagnrho rau cov ntawv thov uas muaj zog thiab corrosion kuj tseem ceeb heev, xws li aerospace thiab marine industries.
Qib 5 (Ti-6Al-4V): Kuj hu ua Ti-6-4 lossis Ti6Al4V, qhov no yog cov titanium alloy feem ntau siv. Nws muaj zog ntau dua li cov khoom lag luam ntshiab, thiab nws kuj muaj kev tiv thaiv corrosion zoo heev. Qib no tsim nyog rau cov ntawv thov uas xav tau qhov sib piv ntawm lub zog-rau-hnyav, xws li aerospace, tsheb, thiab kev kho mob cog.
Qib 7 (Ti-0.15Pd): Qib no muaj cov khoom siv tib yam li Qib 2 tab sis nrog cov palladium ntxiv, uas ua rau muaj kev tiv thaiv corrosion hauv kev txo thiab oxidizing ib puag ncig. Nws yog qhov zoo tagnrho rau cov chaw ua tshuaj lom neeg, tsim hluav taws xob, thiab kev siv dej hiav txwv.
Qib 9 (Ti-3Al-2.5V): Kuj hu ua Ti-3-2.5, cov hlau no muaj kev sib xyaw ntawm txhuas thiab vanadium. Cov qib no yog lub teeb yuag, muaj zog, thiab corrosion-resistant. Nws muaj qhov zoo ntawm kev ua tau zoo dua qub thiab vuam ntau dua li Qib 5. Nws cov kev siv zoo xws li cov khoom siv ua kis las, dav hlau tubing, thiab hydraulic systems.
Qib 12 (Ti-0.3Mo-0.8Ni): Qib 12 muaj kev tiv thaiv corrosion zoo heev thiab muaj zog ntxiv vim yog qhov sib ntxiv ntawm nickel thiab molybdenum. Qib no yog qhov zoo tagnrho rau kev lag luam tshuaj lom neeg, cov khoom siv hluav taws xob, thiab cov hlab ntsha siab.