Qhov ntev thiab qhov tshwj xeeb ntawm lub nkoj molybdenum tuaj yeem sib txawv nyob ntawm cov chaw tsim khoom thiab cov ntawv thov tshwj xeeb. Txawm li cas los xij, qee qhov dav dav thiab qhov tshwj xeeb rau cov nkoj molybdenum yog:
Ntev: feem ntau yog li ntawm 10 hli mus rau 150 hli
Dav: feem ntau yog li ntawm 5 hli mus rau 40 hli
Qhov siab: feem ntau yog li ntawm 3 hli mus rau 20 hli
Phab ntsa thickness: feem ntau yog nyob ntawm {{{0}}.1 hli txog 2.0 hli
Purity: tuaj yeem nyob ntawm 99.95 feem pua rau 99.99 feem pua
Melting point: 2,620 degree (4,748 degree F)
Qhov ceev: 10.2 g / cm³
Thermal conductivity: 138 W / m·K
Hluav taws xob conductivity: 28% IACS (International Annealed Copper Standard)
Nws yog ib qho tseem ceeb uas yuav tsum nco ntsoov tias cov kev qhia tshwj xeeb no tuaj yeem sib txawv nyob ntawm cov chaw tsim khoom tshwj xeeb thiab daim ntawv thov. Nws raug nquahu kom paub meej tias qhov ntev thiab qhov tshwj xeeb nrog cov chaw tsim khoom lossis tus neeg muag khoom ua ntej yuav khoommolybdenum nkoj.