Dab tsi yog qhov txawv ntawm titanium gr2 thiab gr5 titanium hlau?

Aug 09, 2023

Qhov sib txawv ntawm titanium gr2 thiab gr5 titanium hlau:

Composition (Percentage by Luj) Qib 2 Titanium (GR2) Qib 5 Titanium (GR5)
Titanium (Ti) Kwv yees li 99.2 feem pua Kwv yees li 90 feem pua
Aluminium (Al) - Kwv yees li 6 feem pua
Vanadium (V) - Kwv yees li 4 feem pua
Hlau (Fe) Qhov siab tshaj plaws 0.3 feem pua Ntau tshaj 0.25 feem pua
Cov pa oxygen (O) Ntau tshaj 0.25 feem pua Ntau tshaj 0.2 feem pua
Cov pa roj carbon (C) Ntau tshaj 0.1 feem pua Ntau tshaj 0.08 feem pua
Nitrogen (N) Ntau tshaj 0.03 feem pua -
Hydrogen (H) Ntau tshaj 0.015 feem pua -
Lwm Yam Khoom Cov lej Taug qab tus nqi ntawm lwm yam impurities

Lub zog thiab Mechanical Properties:

GR2 titanium hlau muaj ductility zoo, zoo heev formability, thiab impressive corrosion kuj. Txawm li cas los xij, nws muaj zog qis dua piv rau GR5 titanium.

buy ER Ti-2 ER titanium filler wire
GR5 titanium hlaumuaj lub zog-rau-qhov hnyav piv, ua rau nws muaj zog thiab ruaj khov dua GR2. Nws cov khoom siv kho tshuab, suav nrog lub zog tensile, lub zog tawm los, thiab hardness, yog qhov siab dua.

Kev kho cua sov:

GR2 titanium hlau tuaj yeem ua haujlwm txias lossis ua kom zoo dua los txhim kho cov khoom tshwj xeeb, xws li muaj zog ntxiv lossis txhim kho ductility.
GR5 titanium hlau tuaj yeem raug kho cua sov kom ua tiav cov txheej txheem sib txawv thiab cov khoom, suav nrog kev muaj zog ntxiv, txhim kho kev qaug zog, thiab kev nkag siab zoo dua.

Daim ntaub ntawv: Vim nws zoo heev corrosion kuj thiab formability, GR2 titanium hlau pom daim ntaub ntawv nyob rau hauv industries xws li tshuaj ua, marine khoom, desalination, thiab architectural daim ntaub ntawv.
GR5 titanium hlau lub zog muaj zog thiab qaug zog ua rau nws tsim nyog rau cov khoom siv hauv aerospace, cov khoom siv hauv tsheb, cov khoom siv tshuaj biomedical, thiab cov khoom ua si uas yuav tsum tau hnav tsis tau cov khoom siv.

ERTi-1 ER Ti-2 ER Ti-5 ER Ti-7 ER Ti-9 ER Ti-12 titanium filler wire supplier

Tus nqi:

GR2 titanium hlauyog feem ntau pheej yig dua piv rau GR5 titanium hlau, feem ntau vim nws yooj yim muaj pes tsawg leeg thiab cov txheej txheem ntau lawm.
Hauv cov ntsiab lus, thaum ob qho tib si GR2 thiab GR5 titanium xov hlau muaj kev tiv thaiv corrosion zoo heev, txhua qib muaj cov khoom tshwj xeeb uas ua rau lawv haum rau cov ntawv thov tshwj xeeb. GR2 paub txog nws txoj kev tsim, ductility, thiab corrosion kuj, thaum GR5 muaj zog dua, kev qaug zog zoo dua, thiab ntau yam kev siv hauv kev lag luam aerospace, automotive, thiab biomedical industries.