Dab tsi yog qhov txawv ntawm titanium qhov (socket) lub taub hau hau ntsia hlau 10-24 UNC thiab 10-24 UNC 3A?

May 08, 2024

10-24UNC yog ib qho American unified nti xov, qhov loj yog 10 #, xov txoj kab uas hla yog 4.826mm, thiab hauv qab lub qhov taub yog 3.960mm, UNC sawv cev rau American coarse xov, 10-24UNC, thiab UNC 3A tsuas yog sib txawv ntawm qhov tseeb, tab sis qhov loj me yog tib yam.

ASME B 183 - 2012 Gr2 titanium shoulder bolt

Yuav ua li cas peb sib txawv ntawm UNC thiab UNF threads?
1. Txawv thicknesses:
unc yog ib tug ntxhib xov, thiab unf yog ib tug zoo xov.
2. Ntau qhov sib txawv:
unc coarse xov M8, suab P=1.25, unf xov zoo M8, suab P=1
3. Ntau txoj kev sau npe:
unc coarse xov series: 3/8-16UNC-2A, unf fine thread series: 3/8-24UNF-2A (xov txoj kab uas hla-ntau ntawm threads ib nti series code - qib precision).

Gr2 DIN912 titanium socket head cap screw M6x30

Cov ntaub ntawv txuas ntxiv:
1. UN xov yog cov qauv threaded raws li imperial qhov ntev sib koom ua ke los ntawm Tebchaws Meskas, Tebchaws Askiv, thiab Canada. Nws yog hu ua ib txoj xov sib koom ua ke thiab feem ntau hu ua American xov.
2. American xov: coarse xov series UNC, nplua xov series UNF, ntxiv zoo xov series UNEF, taag suab series UN.

DIN912 Gr2 titanium socket head cap screw M6x20

Yog xav paub ntxiv txog Asmeskas ua titanium screws thiab hexagon socket taub hau titanium bolts, tsis txhob yig tau tiv tauj nrog peb cov kws tsim khoom muag.

Cov ntaub ntawv tiv tauj:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Xa kev nug