Nickel crucible yog lub thawv sim ua los ntawm cov nickel ntshiab lossis npib tsib xee alloy nrog kub oxidation tsis kam. Ni200 npib tsib xee crucible yog ua los ntawm cov khoom zoo siab nickel raw khoom, ua los ntawm kev tig thiab milling nickel rods, los yog stamped los ntawm npib tsib xee daim hlau (nyias phab ntsa crucible). Nickel alloy crucible yog ua raws li cov nickel ntshiab, thiab qee cov ntsiab lus alloy ntxiv los txhim kho nws cov hardness, toughness thiab corrosion kuj.
Txij li cov npib tsib xee crucible tau zoo heev kub-kub oxidation tsis kam thiab tshuaj stability, nws yog dav siv nyob rau hauv high-temperature smelting thiab cua sov thwmsim nyob rau hauv lub chaw soj nstuam, xws li kub-kub oxide txo, sulfide npaj, carbide npaj, thiab lwm yam. kuj tseem siv tau rau hauv ntau qhov chaw xws li graphite tshuaj vapor deposition thiab kub kub sim ntsuas.
FAQ
Q: 1. Lub nickel crucible tuaj yeem tiv taus kub npaum li cas?
Q: 2. Dab tsi yog kev ceev faj rau kev siv nickel crucible thaum yaj cov qauv?
Kev cuam tshuam ntawm cov ntsev ntsev: Molten hlau ntsev xws li Al, Zn, Pb, Sn, thiab Hg tuaj yeem ua rau nickel crucibles nkig, thiab borax tsis tuaj yeem yaj hauv nickel crucibles.
Q: 3. Yuav ua li cas hlawv nickel crucibles rau xiav-ntsuab?
Thib ob, ntxuav: Tom qab hlawv, boil rau ib ntus nrog 1:20 hydrochloric acid (HCl), thiab tom qab ntawd yaug nrog dej. Cov kauj ruam no ua kom lub crucible huv si thiab npaj rau kev siv tom ntej.
Ua ke, ob kauj ruam no xyuas kom meej tias cov nickel crucible huv si thiab npaj ua ntej siv, ua kom nws zoo dua rau cov kev sim tom ntej lossis cov txheej txheem melting.
Yog xav paub ntxiv txog ni200 nickel hlau nqi thiab customized nickel hlau, thov cuag nrog peb cov kws muag khoom muag.