Daim ntawv thov ntawm titanium alloy nyob rau hauv biomedical teb qhia tau hais tias kev loj hlob sai. Ua ke nrog kev tshawb fawb hauv tsev thiab txawv teb chaws, nws txoj kev txhim kho yav tom ntej yog raws li hauv qab no:
(1) Cov khoom siv lead ua ib leeg tau txais los ntawm ib leeg-crystal biomedical titanium alloy loj hlob nyob rau hauv ib qho kev taw qhia, Elastic modulus nyob ze ntawm tib neeg cov pob txha muaj, thiab fabricated implants kuj yuav muaj zoo elastic modulus txuam;
(2) Ultrafine grained low elastic modulus, siab zog titanium alloy biocompatibility, thiab industrialization;
(3) Kev tswj cov ntaub so ntswg cov khoom ntawm superelastic thiab zoo li lub cim xeeb kev kho mob uas tsis tshua muaj elastic modulus titanium alloys;
(4) Qhov loj ntawm porosity yog kho kom txo tau cov elastic modulus ntawm biomedical ntxeem tau titanium alloy cov ntaub ntawv thaum elevating lawv txhua yam khoom.