2024.4.26 Baoji Fairy Titanium Industry Co., Ltd. xa ERTi12 titanium hlau 2.5mm mus rau Ltalis thiab Netherlands.

gr12 titanium wire
Yuav ua li cas xaiv titanium vuam hlau?
Thaum xaiv titanium alloy vuam hlau, koj yuav tsum xav txog cov kev xav tau zoo xws li cov khoom siv ntawm cov khoom yuav tsum tau welded, kev siv cov kev cai, cov txheej txheem vuam, thiab lwm yam. Feem ntau hais lus, kev xaiv ntawm vuam hlau yuav tsum ua raws li cov hauv qab no:
1. Cov muaj pes tsawg leeg zoo ib yam li cov khoom siv yuav tsum tau welded. Qhov no ua kom cov vuam zoo thiab kev sib koom ua haujlwm.
2. Xaiv cov vuam hlau sib txawv ntawm cov khoom sib txawv thiab cov diameters raws li cov txheej txheem sib txawv. Piv txwv li, rau welding tuab-walled qhov chaw, ib tug vuam hlau nrog ib tug loj txoj kab uas hla yuav tsum tau xaiv.

gr12 titanium welding rod
3. Xav txog cov ntsiab lus impurity thiab nto zoo ntawm cov vuam hlau. Cov ntsiab lus impurity thiab tsis zoo ntawm qhov chaw yuav cuam tshuam rau vuam zoo thiab kev sib koom ua haujlwm.
4. Xaiv cov vuam hlau ntawm qhov sib txawv hardness raws li qhov xav tau tiag tiag. Lub hardness siab dhau yuav txo qhov weldability, thiab tsawg dhau qhov hardness yuav txo qhov hnav tsis kam.

gr12 titanium filler wire
Titanium alloy vuam hlau muaj qhov zoo corrosion kuj nyob rau hauv feem ntau cov xov xwm, tsis yooj yim rau xeb, tuaj yeem tiv taus cov khoom loj, thiab tuaj yeem ua tau yooj yim txiav, tig, thiab lwm yam kev ua haujlwm. Nws yog dav siv hauv aerospace, tsheb, tshuaj lom neeg kev lag luam, thiab lwm yam.