Tsev > Xov xwm > Ntsiab lus

Gr2 ASME B 18.3 ANSIB18.3 UNC 10-32 Titanium Ntsia Hlau Xa Rau Cov Neeg Siv Khoom

Sep 14, 2024

Thaum lub Cuaj Hlis 12, 2024, Baoji Fairy Titanium Co., Ltd. tau xa 10, 000 titanium screws mus rau Tebchaws Meskas. Cov khoom xa tuaj suav nrog hexagon socket taub hau titanium screws thiab titanium lub xub pwg screws, tag nrho cov uas yog British UNC ntshiab titanium screws.

UNC 10-32 titanium screws

Hexagon socket titanium screws, tseem hu ua hexagon socket titanium bolts, thiab khob taub hau titanium screws, hu ua txawv, tab sis lawv txhais tau tias tib yam. Titanium lub xub pwg screws yog ib qho uas nquag siv fastener, uas muaj cov xov ib feem thiab ib lub xub pwg. Lub xub pwg yog ib qho cylindrical protrusion, feem ntau yog siv rau qhov chaw thiab kev txhawb nqa. Lub threaded ib feem txuas ob los yog ntau qhov chaw kom lawv nruj nreem. Qhov zoo ntawm lub xub pwg titanium screws yog tias lawv tuaj yeem txo cov naj npawb ntawm cov khoom thiab lub sijhawm sib dhos, thiab txhim kho kev sib dhos ua haujlwm thiab ua haujlwm zoo.

Gr2 Titanium Socket head cap screw price

Cov qib zog ntawm titanium screws feem ntau tuaj yeem muab faib ua 8.8, 10.9, thiab 12.9. Cov qib no tau muab faib ua raws li cov qauv thoob ntiaj teb, qhov twg qib 8.8 titanium alloy screws yog tsim rau cov xwm txheej uas tsis xav tau lub zog siab. Hauv qhov sib piv, qib 10.9 thiab qib 12.9 titanium alloy screws yog qhov zoo tagnrho rau cov ntawv thov uas xav tau lub zog ntau dua. 12

Lub zog qib ntawm titanium screws feem ntau yog nyob ntawm nws cov khoom thiab kev tsim khoom. Cov khoom siv titanium alloy feem ntau suav nrog Gr1, Gr2, Gr5, thiab lwm yam. Kev xaiv ntawm cov ntaub ntawv no yuav cuam tshuam rau lub cev thiab lub zog ntawm cov ntsia hlau, suav nrog lub zog. Cov txheej txheem tsim khoom kuj tseem cuam tshuam rau lub zog, suav nrog kev kho cua sov, kev kho saum npoo, thiab lwm yam.

14 10-24 UNC Titanium shoulder bolt

Txawm hais tias titanium screws yuav muaj zog me ntsis dua li cov hlau zoo tib yam, lawv muaj kev tiv thaiv corrosion zoo dua thiab hnav cov yam ntxwv. Cov yam ntxwv no ua rau titanium screws muaj qhov tshwj xeeb daim ntawv thov nqi hauv ntau qhov chaw, tshwj xeeb tshaj yog nyob rau hauv cov xwm txheej uas yuav tsum tau hnav thiab corrosion kuj.

Yog xav paub ntxiv txog titanium ntsia hlau nqi, titanium bolt qauv, thiab titanium ntsia hlau lub zog, thov sab laj nrog peb cov kws muag khoom.

UNC Gr2 10-32 titanium screws

Cov ntaub ntawv tiv tauj:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email:sales@tmsalloy.com