DAT57M high-strength titanium alloy uas tsis muaj vanadium keeb tsim los ntawm Daido Steel Ltd. ntawm Nyiv tau ua tiav rau hauv American ASTM B348 / B348M tus qauv (Standard Specification rau Titanium thiab Titanium Alloy Bars thiab Billets), thiab qib sau npe yog qib 41 .
DAT57M titanium alloy yog tsim los ntawm Ti-6Al-1Fe, belongs rau ntxiv rau Titanium alloy. Nws lub ntiajteb txawj nqus yog 4.39, me ntsis qis dua 4.43 ntawm Ti-6Al-4V alloy; Lub zog tensile, qaug zog, thiab lwm yam khoom siv nrog rau kev tsim kub thiab kev ua haujlwm zoo sib npaug ntawm Ti-6Al-4V alloy thiab tsis muaj vanadium, Nws yuav tsum tau hloov cov dav siv Ti-6Al-4V Alloy yav tom ntej.