Titanium Ingot Direct Rolling Cogging

Sep 14, 2022

Titanium thiab titanium alloy ingotdirect dov cogging tau ua tiav tiav nyob rau hauv Suav teb, thiab cogged zoo tshaj theem ntawm ceev forging billet.

Piv nrog rau ntau qhov kub forging, titanium ingot ncaj dov muaj 3 qhov zoo: lub ingot yog ncaj qha dov mus rau hauv lub kub billet, txuag roj noj. Noj 3 tons ntawm lub tshuab nqus tsev nqus khoom noj khoom haus ua piv txwv, lub sij hawm noj ncaj qha dov tsuas yog 7.5 feem pua ​​​​ntawm cov forging ceev, uas ua rau muaj txiaj ntsig zoo; Cov txheej txheem dov muaj qhov ntsuas kub me me, muaj zog deformation txuas ntxiv, tsis muaj qhov cuam tshuam ntawm qhov chaw, thiab tawg, thiab txhim kho qhov zoo ntawm titanium ingots tom qab ua tiav.

Tam sim no, cov txheej txheem ncaj qha dov coggging yog cov thev naus laus zis tshaj plaws hauv kev ua haujlwm ntawm titanium thiab titanium alloy pas nrig thiab hlau dov. Txog xyoo 2021, ib lub lag luam hauv Suav teb yuav nqis peev ntau los ua tus thawj coj.

Titanium ingot direct rolling cogging

Xa kev nug