Titanium yeeb nkab yog ib hom yeeb nkab tshiab hauv xyoo tas los no. Vim nws muaj cov yam ntxwv ntawm lub teeb yuag, siab zog, muaj zog corrosion-kuj, thiab qis-kub tsis kam, nws yog feem ntau siv rau hauv cov txheej txheem uas lwm cov kav dej tsis muaj peev xwm.
Titanium raj yog ua los ntawm TA1 thiab TA2 muaj ntshiab titanium. Qhov ntsuas kub siv tau yog -140 250 degree. Thaum qhov kub siab tshaj 250 degree, nws cov khoom siv tshuab yuav poob qis.
Qhov kev qhia tshwj xeeb ntawm cov yeeb nkab titanium yog 20 400mm nominal txoj kab uas hla. Nws muaj feem xyuam rau qhov siab qis thiab nruab nrab. Phab ntsa tuab ntawm qhov qis- cov yeeb nkab siab yog 2.8 12.7mm, thiab phab ntsa tuab ntawm cov yeeb nkab nruab nrab siab yog 3.7 21.4mm.
Txawm hais tias titanium yeeb nkab muaj ntau qhov zoo, nws tsis tau siv dav vim nws cov nqi siab thiab vuam nyuaj.