Khoom Taw Qhia
1. Gr2 titanium ntawvyog cov ntawv hlau ua los ntawm titanium qib 2, Asmeskas tus qauv yog ASTM B265, ASTM F136, ASTM F67, AMS4928
2. Cov ntaub ntawv tseem ceeb:
US Qib: Gr1, Gr2, Gr3, Gr5, Gr7, Gr11, Gr12, BT1-00, BT1-0, thiab lwm yam.
Lavxias tus qauv Qib: BT1-00, BT1-0, BT1-2, thiab lwm yam.
Titanium ntawv loj: T x W x L (mm)
Thickness: 4. 1-60 0 hli
Dav: 400-3000mm x Length 1000-4000mm Kub Rolling
Nyias titanium ntawv
Thickness: {{0}} 3-4.0mm x Dav 400-1500mm x Length 1000-3000mm Txias dov
Hardness: HB{0}}HB340
| npe khoom | Titanium thiab titanium alloy phaj | tuab | 0 3-60MM |
| cov khoom siv | Ntshiab titanium, titanium alloy | Dav ntev | tuaj yeem txiav thiab kho |
| Qib khoom | Gr1 / Gr2 / Gr12 / Gr9 / Gr5 thiab lwm yam. | daim ntawv thov | Industrial, kho mob |
| Cov xwm txheej muab khoom | Kub-ua hauj lwm, txias ua hauj lwm, annealing, solid tov | Cov khoom siv txheem | ASTMB265, ASTMF136, ASTMF67 thiab lwm yam. |
3. Titanium sheet hlau daim ntawv thov:aviation, tshuaj, roj av, machinery, kho mob thiab lwm yam lag luam.
Titanium hlau tau dhau los ua ib qho ntawm cov khoom siv tiv thaiv corrosion tseem ceeb hauv cov khoom siv tshuaj thiab tau tsim nws txoj haujlwm tiv thaiv corrosion hauv cov khoom siv tshuaj. Raws li cov khoom siv zoo tshaj plaws hauv cov khoom siv tshuaj, titanium kuj tau nyiam ntau thiab ntau dua los ntawm engineers thiab cov kws tshaj lij.
Qhia nthuav dav


4. Titanium sheet manufacturing txheej txheem
Kub forging yog txheej txheem forging ua tiav saum cov hlau recrystallization kub.
Kub dov ntawm Gr2 titanium daim ntawv yog txheej txheem dov ua haujlwm ntawm qhov kub siab tshaj qhov kub ntawm recrystallization, thiab txias dov yog txheej txheem dov ntawm cov yas deformation kub.
Annealing: nws yog cov txheej txheem kev kho cua sov hlau, maj mam ua kom sov cov hlau mus rau qhov kub thiab txias, ua kom lub sijhawm txaus, thiab tom qab ntawd txias nws ntawm qhov tsim nyog ceev (feem ntau qeeb txias, qee zaum tswj kom txias).
Pickling: Muab cov khoom tso rau hauv qhov sib xyaw ntawm hydrofluoric acid thiab nitric acid kom tshem tawm cov oxides thiab lwm cov yeeb yaj kiab ntawm cov hlau. Nws yog kev kho mob nruab nrab lossis pretreatment ntawm electroplating, dov, enamel, thiab lwm yam txheej txheem.
5. Peb qhov zoo
Tom qab xyoo ntawm kev nce qib, titanium thiab nws cov alloys tau siv dav hauv kev tsim tshuaj raws li cov khoom siv zoo heev corrosion-resistant. Tam sim no, daim ntawv thov ntawm cov khoom siv titanium tau nthuav dav los ntawm thawj zaug soda tshauv thiab caustic soda industries mus rau chlorate, ammonium chloride, urea, organic synthesis, dyes, inorganic ntsev, tshuaj tua kab, hluavtaws fibers, chiv, thiab tshuaj zoo. Me me, ib qho kev loj hlob mus rau loj, muaj ntau haiv neeg.
Cov txiaj ntsig ntawm kev tshawb fawb ntawm cov khoom siv hluav taws xob tau pom tias cov khoom siv hluav taws xob titanium suav txog 57 feem pua, titanium anodes suav txog 20 feem pua, titanium cov hlab ntsha suav txog 16 feem pua, thiab lwm yam suav txog 7 feem pua. Hauv kev lag luam tshuaj, "ob alkalis" yog cov khoom tseem ceeb, thiab cov khoom siv hluav taws xob titanium tau siv ntau tshaj plaws hauv cov khoom siv tshuaj.
Raws li tus kws tshaj lij titanium ntawv xa khoom, txij li thaum tsim lub tuam txhab, nws tau tsom mus rau titanium hlau teb tau ntau xyoo thiab tau ntsib ntau txoj kev lag luam thiab ntau cov txheej txheem corrosion-resistant kev daws teeb meem, tau txais kev nplua nuj nyob hauv cov khoom tsim thiab kev tsim khoom, thiab txuas ntxiv tsim kho tshiab los coj cov neeg siv khoom tuaj rau ntau yam kev pabcuam thiab kev paub dhau los.
Cim npe nrov: gr2 titanium ntawv, lwm tus neeg, manufacturers, hoobkas, nqe, tej, kev muag, Tshuag, yuav luv nqi