Yuav ua li cas xaiv cov kev ntsuam xyuas tsis zoo ntawm cov khoom titanium

Jan 14, 2022

Yuav ua li cas xaiv cov kev ntsuam xyuas tsis zoo ntawm cov khoom titanium

1. Raw khoom tshuaj xyuas

1) Daim ntawv: UT

2) Forgings thiab tuav: UT, MT, PT

3) Cov kav dej: UT (RT), MT (PT)

4) Bolt: UT, MT (PT2)

2. Kev tshuaj xyuas vuam

1) Groove txoj haujlwm: UT, PT (MT)

2) Welded ntu: PT (MT)

3) Lub taub hau vuam: RT (UTD), MT (PT)

4) Fillet welds thiab T-welds: UT (RT), PT (MT)

3. Lwm yam kev tshuaj xyuas

1) Cov cuab yeej fixture weld caws pliav MT (PT)

2) Cov khoom siv sib xyaw, kev tshawb nrhiav cov txheej txheem sib xyaw, cov txheej txheem tawg tawg: UT

3) Cov khoom siv sib xyaw ua ke nrhiav kom pom, ntog txheej txheej, ua ntej surfacing: MT (PT)

4) Cov khoom siv sib xyaw ua ke nrhiav pom, ntog txheej txheej, tom qab ntog: UT, PT

5) Tom qab kuaj hydrostatic: MT