Nickel Hlau 0.025mm

Nickel Hlau 0.025mm

nickel hlau 0.025mm
nickel 200 hlau
nickel hlau nqi
ntshiab nickel hlau
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

 

Khoom Taw Qhia

1. Nickel xaim 0.025mm yog cov hlau hlau ua los ntawm cov npib tsib xee, uas yog cov hlau nplaum dawb ntawm ib lub spool.

2. Cov ntaub ntawv yooj yim

Qib: Nickel 200, Nickel 201 (UNS N02200, UNS N02201)

Txuj: ASTM B166

Txoj kab uas hla: {{0}} {{0}}. 0.5mm, 0.6mm thiab lwm yam.

Melting point 1446 degrees Celsius

Qhov ceev 8.89 g / cm3

Nickel 200 yog npib tsib xee ntshiab nrog kev ua tau zoo thiab zoo alkali corrosion kuj (xws li sodium hydroxide). Nws kuj muaj lub zog zoo txhua yam, corrosion kuj, thiab kub ua hauj.

Qhia nthuav dav


nickel 200 wire

nickel 200 hlau

pure nickel wire

ntshiab nickel hlau

3. Nickel hlau 0.025mm daim ntaub ntawv: hlau-qhov txhab resistors, hluav taws xob cua sov, cua sov daim hlau, hluav taws xob cua sov coils, shunts rau me me khoom siv hauv tsev (hluav taws xob kettles, kas fes lauj kaub, toasters, thiab lwm yam), precision kuj Cheebtsam, high-temperature-resistant xov hlau thiab cables rau hlau-qhov txhab resistors, txhuas hlau nyob rau hauv kev twb kev txuas ntawm cua sov caij, high-temperature nickel plating, ceramic cua sov daim hlau, kub sensing hlau, ntsuas kub ntsuas hlau.

4. Nickel hlau 0.025mm tshuaj lom neeg raws li ASTMB160

Cov khoom siv tshuajNickel minCu maxFe maxMn maxC maxSi maxS max
Nickel (UNSN02200)990.250.40.350.150.350.01
Low-C npib tsib xee (UNS N02201)990.250.40.350.020.350.01

Cim npe nrov: nickel hlau 0.025mm, lwm tus neeg, manufacturers, hoobkas, nqe, tej, muag, hauv Tshuag, yuav luv nqi