Khoom Taw Qhia
1. BT9 titanium puag ncig baryog Russia-qib titanium alloy bar, uas yog ib qho ntawm cov feem ntau lug siv high-temperature titanium alloy qib nrog lub siab tshaj plaws kev khiav hauj lwm kub ntawm 500 degree C.
2. BT9(VT9) titanium bar muaj qhov loj thiab cov qauv
OD: 6.0 ~ 500mm lossis tus neeg siv khoom loj
Txheem: ΓOCT26492-85 ASTM B348-2005 DIN17862-1990 DIN17864-1993
3. Nta ntawm BT9 titanium bar
Ti-6.5Al-3.5Mo-1.5Cr-0.3Si
Nws yog ib hom titanium alloy tshav kub-resistant titanium alloy nrog cov txhuas sib npaug ntawm 6.5 thiab molybdenum sib npaug ntawm 3.5, nws lub zog tensile siab dua Gr5, nrog kev ua haujlwm kub kub (cov txheej txheem ua tau zoo thiab superplasticity), nws tuaj yeem welded thiab machined. sib txawv.


4. Tshuaj muaj pes tsawg leeg ntawm VT9 titanium puag ncig pas nrig
| Qib | Cov tshuaj muaj pes tsawg leeg (feem ntau) (feem pua ) tsis ntau dua (tshwj tsis yog rau cov nqi teev tseg) | ||||||||||||||
| Ti | Al | Cr | Mo | Sn | Mn | V | Fe | Si | Zr | C | N | H | O | qhov sum ntawm lwm yam | |
| BT9 (VT9) | puag | 5.8~7.0 | — | 2.8~3.8 | — | — | — | 0.25 | 0.2~0.35 | 1.0~2.0 | 0.1 | 0.05 | 0.015 | 0.15 | 0.3 |
5. Dab tsi yog daim ntawv thov ntawm BT9 titanium round bar?
VT9 titanium round pas nrig yog dav siv los ua lub dav hlau tshuab compressor cov khoom xws li discs, hniav, nruas, thiab shafts. cov khoom kuj tuaj yeem ua rau tshwj xeeb-puab castings.
6. Ntim thiab xa khoom
Peb muab cov txheej txheem export ntim, sab hauv yog pearl paj rwb thiab ua npuas ncauj zaj duab xis los txo qhov cuam tshuam thiab kev sib txhuam ntawm cov khoom thauj. Cov khoom qis dua 10kg feem ntau tau ntim rau hauv thawv.
Peb muaj cov tuam txhab xa khoom mus sij hawm ntev xws li FedEx, DHL, TNT, UPS, thiab lwm yam.
Hauv huab cua thiab hiav txwv shipping, peb ib txwm xaiv kev nyab xeeb thiab ceev thoob ntiaj teb txoj kev, peb ib txwm xaiv cov kev nthuav qhia sib txawv raws li cov neeg siv khoom hauv ntau lub teb chaws kom txuag tau cov nqi rau cov neeg siv khoom.

7. Peb qhov zoo
Peb BT9 titanium round bar tsim nyob rau hauv Baoji, tshwj xeeb hauv kev tsim titanium nrog xyoo dhau los ntawm kev xa tawm, peb cov khoom raug muag rau Asia, Europe, North America, thiab Kauslim Teb, Txhua yam khoom peb tsim yog raws li tus qauv: German txuj, Aerospacestandard, Cov txheej txheem European, thiab lwm yam, suav nrog ANSI / ASTM, JIS, DIN, thiab lwm yam.
8. Qhov twg yuav VT6 titanium round bar?
Hu rau peb kom tau txais BT9 Titanium wrought alloy bar nqe lossis xa tuaj rau peb ntawm sales@tmsalloy.com rau cov lus hais, peb yuav zoo siab nrog koj tham txog koj cov lus nug.
Cim npe nrov: bt9 titanium round bar, lwm tus neeg, manufacturers, hoobkas, nqe, tej, kev muag, Tshuag, yuav luv nqi