Universal titanium alloy 6AL-4V (ELD) zoo ib yam li hom 6AI-4V hauv kev tshuaj xyuas tshuaj tshwj tsis yog rau cov roj qis qis qis (ELI) Los ntawm kev tswj cov pa paug no, qhov ua kom muaj zog ntawm cov pob qij txha tau nce ntxiv. Alloy 4956 yog siv los txuas cov kua hydrogen tankage thiab airframe qhov chaw uas yuav tsum tau muaj lub siab tawg toughness
Cov tshuaj muaj pes tsawg leeg sib txawv
| Cov qauv | Al | V | C | H | Fe | N | O | Lwm yam |
| TIAB SA 4956 | <=6.75 | <=4.5 | <=0.03 | <=0.005 | <=0.2 | <=0.012 | <=0.08 | <0.1 |
| AWS 5.16 | 5.5~6.75 | 3.5~4.5 | <=0.05 | <=0.015 | <=0.22 | <=0.03 | 0.12~0.2 | - |

Mechanical properties/Mpa (chaw kub) yuav luag zoo ib yam
| Tensile zog | 896 |
| Yield | 827 |
| Elongation | 10% |
Qhov tseem ceeb tshaj plaws yog AMS 4956 muaj qhov xav tau ntawm cov khoom siv hluav taws xob qis
Mechanical zog/Mpa -196 degree
| Tensile zog | 1500 |
| Yield | 1390 |
| Elongation | 14% |
Yog xav paub ntxiv txog 6Al4V Eli titanium hlau, thiab titanium vuam hlau, thov hu rau peb tus kws muag khoom muag.