Cold-Rolled Molybdenum Sheet for Sale

Cold-Rolled Molybdenum Sheet for Sale

Molybdenum is hard and soft and is more ductile than tungsten. Molybdenum has high elastic modulus and is mainly used for molybdenum electrodes, vacuum furnaces, etc
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

 

Basic Info

Model NO. Mo-1
Density 10.2g/Cc
Specification Range as Per Customer's Request
Melting Point 2623
Surface Cold-Rolled, Polished, Black
Processing Technique Forging, Hot-Rolling, Cold-Rolling
Property Good Corrosion Resistance, Thermal Conductivity
Working Temperature 1100~1800
Certification ISO 9001
Tensile Strength 610MPa
Elongation More Than 10%
Glossiness Ra0.6-3.2
Transport Mode Express, by Air, by Sea
Lead Time Depend on Quantity(7-25days)
Port Qingdao Tianjin Shanghai Beijing
Sample Available
Transport Package Standard Export Package
Specification As per the customer's request
Origin Baoji, Shannxi, China
HS Code

8102950000

Molybdenum sheet in stock

Product Description

Grade: Mo1 Mo2

Molybdenum content 99.95%~99.6% Impurity content≤ 0.04%

The density of molybdenum in molybdenum plates is 10.2 g/cm3

Surface: black, alkaline washing, polishing

Standards: GB/T 3876-2007 (molybdenum and molybdenum alloy plate), GB/T 3877-83 (molybdenum foil), ASTM B386-91 (molybdenum and molybdenum alloy plate, sheet, strip and foil)

Processing Flow

We adopt a proprietary production process, and the hot and cold-rolled high-temperature molybdenum plates, sheets, and strip products produced by rolling increase the crystallization temperature of molybdenum by 500 °C ~ 700 °C to meet the needs of heat insulation screen materials with a temperature of 1850 °C in the vacuum furnace.

Molybdenum sheet

Molybdenum sheet applications: Molybdenum plate is used in electronics, aviation, aerospace, electric light source, the heating element in vacuum furnace, heat insulation screen, molybdenum boat, molybdenum crucible, etc.

supply Molybdenum sheet Mo1

Our Advantage

FAQ
Q: What information should I let you know if I want to get a quotation?

A: The required material dimension (Thickness*Width*Length,diameter*length; if possible, please kindly supply us drawings).
They required more information, such as Surface Condition, Tolerance Request, Quantity, and other mechanical and technical details.
   
If it is possible, please also provide the application of products, and we will recommend the most suitable products with details for confirmation.

Q: How do you guarantee the quality of the products?

A: Each step of production and finished products will be carried out by inspection by the QC department before storing them in the warehouse. NG goods are not allowed in the completed goods warehouse.

Q: Can you guarantee prompt delivery?

A: Yes, when we get your inquiries, not only we will evaluate the more competitive price, but also we can get the most reasonable delivery time. So prompt delivery can be guaranteed.

Q: What is the shipping cost?

A: The shipping cost is determined by the destination port, weight, packing size, and total CBM of the products, we will try our best to get the most reasonable shipping cost from the forwarders or express couriers to help you save more money.

Q: What is the transportation way?
A: If the Gross Weight is ≤45kg, it's better by express such as TNT, DHL, FedEx, etc.
If the Gross Weight is between 45kg to 100kg, express or by air to your nearest airport can be both considered.
If the Gross Weight is≥ 100kg, you can choose by Air or Sea to the nearest port.

Cim npe nrov: cold-rolled molybdenum sheet for sale, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China