Khoom Taw Qhia
1. Gr12 titanium phajyog nyob ze alpha titanium hlau exhibiting txhim kho lub zog thiab optimum ASMA code tsim, ua ke nrog superior crevice corrosion kuj thiab zoo heev kuj nyob rau hauv oxidizing rau me ntsis txo tej yam kev mob, tshwj xeeb tshaj yog chlorides.
2. Cov ntaub ntawv yooj yim
| npe khoom | Gr12 Titanium phaj | tuab | 0 3-60MM |
| cov khoom siv | Gr12 Ti0.3Mo0.8Ni | Dav | 1000/1200/1220/1500/2000 |
| daim ntawv thov | Kev lag luam | Ntev | tuaj yeem txiav thiab kho |
| Cov xwm txheej muab khoom | Kub-ua hauj lwm, txias ua hauj lwm, annealing, solid tov | Cov khoom siv txheem | ASTM 265 |
Gr12 Tshuaj muaj pes tsawg leeg:
| Qib | N | C | H | Fe | O | Al | V | Pa | Mo | Ni | Ti |
Gr 12 | 0.03 | 0.08 | 0.015 | 0.30 | 0.25 | / | / | / | 0.2~0.4 | 0.6~0.9 | bal |
Ti{0}}.3Mo0.8Ni Tensile zog:
Qib | Tensile zog (min) | Yield zog (min) | Elongation (%) | ||
Ksi | MPa | Ksi | MPa | ||
12 | 70 | 438 | 50 | 345 | 18 |
Qhia nthuav dav

Gr12 titanium phaj

Ti{0}}.3mo0.8ni titanium ntawv
3. Cov nominal muaj pes tsawg leeg ntawm Gr12 titanium ntawv
Titanium molybdenum nickel alloy yog Ti-0.3Mo-0.8Ni, uas yog Ti-12 alloy tshawb fawb thiab tsim los ntawm Tebchaws Meskas hauv nruab nrab-1970s. Nws yog titanium alloy resistant rau crevice corrosion. Lub zog tensile ntawm 300 yog ob zaug ntawm cov ntshiab titanium, corrosion kuj ntawm kev txo cov xov xwm yog pom tseeb, thiab crevice corrosion tsis tshwm sim nyob rau hauv cov tshuaj chloride ntawm 150-200.
4. Kev tsim cov txheej txheem ntawm gr12 titanium phaj
Cov khoom siv raw ntawm Gr12 titanium phaj yog ua tiav titanium phaj tau los ntawm titanium molybdenum npib tsib xee alloy titanium ingot tom qab forging thiab dov thiab tom qab ntawd kho cov nplai oxide. Cov ntsiab lus titanium yog li 98.7 feem pua, 1 feem pua molybdenum nickel alloy (0.3 feem pua Mo, 0.8 feem pua Ni), thiab tus so yog Fe, O, N, H, thiab lwm yam impurity cov ntsiab lus. Tus nqi tsim khoom yog zoo ib yam li cov ntshiab titanium, tab sis cov khoom siv thiab corrosion kuj zoo dua li ntshiab titanium.
5. Daim ntawv thov ntawm Ti0.3mo0.8ni titanium phaj
(Ti-0.3Mo-0.8Ni) Gr12 titanium phaj muaj kev ua haujlwm zoo corrosion rau qhov kub, tsis muaj pH chloride, lossis tsis muaj zog txo cov kua qaub, thiab nws cov corrosion kuj zoo dua li cov ntshiab titanium thiab kaw. rau Gr7 alloy.
6. Peb qhov zoo
Kev cob qha titanium phaj, Gr12 titanium phaj tsum, peb txuas ntxiv txhim kho thiab txhim kho cov txheej txheem kev tswj hwm sab hauv, txhua lub tuam tsev yog lub luag haujlwm rau tag nrho cov xwm txheej thiab hais rau kev cob qhia sab nraud, kev cob qhia sab hauv, thiab kev sib xyaw ntawm kev xav thiab kev xyaum.
Cim npe nrov: gr12 titanium phaj, lwm tus neeg, manufacturers, hoobkas, nqe, tej, kev muag, Tshuag, yuav luv nqi