Gr4 Titanium Bar

Gr4 Titanium Bar

Gr4 titanium puag ncig bar
ASTMB 348 titanium pas nrig
Gr4 titanium bar
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

 

Khoom Taw Qhia

1. Gr4 Titanium bar yog cov khoom siv titanium ntshiab, tab sis nws lub zog siab dua Gr1 ~ Gr3.

2. Cov ntaub ntawv yooj yim

Titanium puag ncig bar specification: dov ¢8.0---40mm × L; forging ¢40---150mm × L

Titanium qws qauv: ASTM 348 ASTM F136, ASTM F67, AMS4928

Nto: dub nto, machining nto, polishing nto (H11, H9, H8)

Titanium bar yog siv tsis tu ncua nyob rau hauv aviation rau nws tsis kam mus corrosion thiab kub, thiab nws siab zog-rau-qhov hnyav piv. Titanium alloys feem ntau muaj zog dua aluminium alloys thaum sib dua li hlau.

Qhia nthuav dav


gr4 titanium rod

Gr4 titanium puag ncig bar

gr4 titanium round bar

Gr4 titanium bar

3. Qib 4 yog unalloyed thiab suav tias yog kev lag luam ntshiab lossis "CP". Feem ntau, lub zog tensile thiab yield zog nce nrog cov lej rau cov qib "ntshiab" no. Qhov sib txawv ntawm lub cev muaj zog feem ntau yog vim muaj cov ntsiab lus ntawm interstitial. Lawv yog siv nyob rau hauv corrosion-resistant daim ntaub ntawv, lub caij no, tus nqi, yooj yim ntawm kev tsim, thiab vuam yog ib qho tseem ceeb heev.

4. Gr4 titanium bar cov tshuaj lom neeg thiab cov khoom siv kho tshuab

tshuaj lom neegNCH FeO Residuals max txhuaResiduals max tag nrho
Gr40.050.080.0150.50.40.10.4
QibTensile zog Mpayield zog Mpaelongation
Gr455048315