Khoom Taw Qhia
1. Tungsten crucible muaj lub siab melting point thiab boiling point, zoo-kub lub zog, hnav tsis kam, thiab corrosion kuj. Nws yog dav siv nyob rau hauv tsawg lub ntiaj teb smelting, quartz iav, siv lead ua kev loj hlob, thiab lwm yam lag luam.
2. Cov ntaub ntawv yooj yim
Tungsten melting point 3410 degree
① purity: W Ntau dua lossis sib npaug rau 99.95 feem pua;
② ceev: Ntau dua lossis sib npaug ntawm 18.5g / cm3;
③ Qhov siab tshaj plaws ntawm daim ntawv thov kub: 2400 degree .
3. Lub zog tensile thiab deformation tsis kam ntawm tungsten crucible tsim los ntawm txoj kev forging yog zoo dua li cov uas ua los ntawm lwm txoj kev.
Forging tungsten crucible tseem ceeb muaj peb kauj ruam: kev npaj dawb paug, forging thiab machining .: dawb paug npaj, forging, thiab machining. Nws qhov ceev yog feem ntau ntau dua 19.0g / cm3, yuav luag ncav cuag qhov theoretical ntom thiab nws txoj kab uas hla feem ntau tsawg dua 100mm.
Qhia nthuav dav

Tungsten crucible

Tungsten crucible rau melting
4. Tungsten crucibles daim ntaub ntawv: sapphire siv lead ua kev loj hlob thiab tsis tshua muaj-lub ntiaj teb melting vim cov yam ntxwv zoo heev.
5. Kev faib tawm thiab purity ntawm tungsten crucible
Forged tungsten crucible (phab ntsa thickness 8-20mm)
| purity feem pua | density Ntau dua los yog sib npaug | qhov loj / mm | kam rau ua/mm | Nto roughness | ||
| Dia | Qhov siab | Txoj kab uas hla | Qhov siab | |||
| 99.95 | 19.35 g/m3³ | 10-500 | 10-750 | ±5 | ±5 | Ra=1.6 |