tungsten nickel hlau pas nrig, tseem hu ua W-Ni-Fe pas nrig, yog ib hom high-density tungsten alloy. Nws yog tsim los ntawm tungsten (85-98 feem pua), npib tsib xee (2-10 feem pua), thiab hlau (05-1.5%), uas ua rau nws yog ib qho kev xaiv zoo rau daim ntawv thov yuav tsum muaj zog, siab ceev, thiab siab tiv thaiv corrosion thiab hnav.
Khoom nta:
Tungsten npib tsib xee-hlau (W-Ni-Fe) rods yog cov khoom siv hluav taws xob zoo tshaj plaws uas paub txog lawv qhov sib xyaw ua ke ntawm lub zog siab, kev ua haujlwm kub zoo, thiab cov khoom siv zoo heev. Qee qhov tseem ceeb ntawm tungsten nickel hlau rods suav nrog:
Kev kub siab: W-Ni-Fe-Fe Rods paub txog lawv lub siab ntom ntom, uas ua rau lawv zoo tshaj plaws rau kev siv, xws li hauv Aerospace, ua tub rog, thiab kev lag luam tsheb.
Cov khoom siv zoo heev: Cov pas nrig no muaj cov khoom siv kho tshuab zoo heev, suav nrog lub zog tensile siab, toughness, thiab tsis kam mus deformation. Lawv kuj tiv taus tawg thiab hnav.
Cov cua kub zoo tshaj plaws: Tungsten nickel hlau rods muaj qhov tshwj xeeb kub tsis kam, tiv taus kub txog li 1, 000 degree . Qhov no ua rau lawv zoo tagnrho rau siv nyob rau hauv high-kub ib puag ncig, xws li foundries, furnace qhov chaw, thiab foob pob ua ntxaij cav nozzles.
Kev ua haujlwm siab rau tshuaj lom neeg corrosion: Cov pas nrig no kuj muaj peev xwm tiv taus tshuaj lom neeg corrosion, ua rau lawv zoo tagnrho rau kev siv tshuaj lom neeg hnyav.
Tsawg thermal expansion: Tungsten nickel hlau rods muaj qhov thermal expansion, uas txhais tau hais tias lawv yuav tsis nthuav los yog cog lus loj thaum raug tshav kub los yog txias.

Specification Tel: 0917-3664600
| Qib | Tungsten Nickel Hlau Alloy (W-Ni-Fe) |
| Loj | 0.125 nti rau 1 nti X 6 nti rau 12 nti ntev |
| Nto | polishing ci nto |
| Cov qauv | ASTM B777 Cov khoom lag luam |
Lub Hoobkas ncig saib Tel: 0917-3664600



Khoom thiab tsim cov txheej txheem ntawm tungsten nickel hlau alloy bar Tel: 0917-3664600
Tungsten nickel hlau rods muaj qhov ceev ntawm 17.5-18.75 g / cm³, uas yog mus txog 70 feem pua denser dua txhuas. Qhov no ua rau lawv zoo tagnrho rau siv rau hauv cov ntawv thov uas yuav tsum muaj qhov hnyav thiab ntim me me, xws li hauv aerospace, hluav taws xob tiv thaiv, thiab khoom siv kho mob.
Hais txog cov khoom siv kho tshuab, WNiFe rods muaj lub zog tensile ntawm 600-1000 MPa thiab lub zog tawm ntawm 400-800 MPa. Lawv kuj muaj kev hnav zoo heev, ua rau lawv zoo tagnrho rau kev siv hauv cov cuab yeej thiab cov khoom siv tshuab uas raug kev ntxhov siab thiab kev sib txhuam.
Tungsten npib tsib xee hlau rods feem ntau yog tsim los ntawm cov hmoov hlau metallurgy cov txheej txheem, qhov twg cov hmoov ntawm tungsten, npib tsib xee, thiab hlau yog sib xyaw ua ke, compacted rau hauv ib qho kev xav, thiab tom qab ntawd sintered ntawm qhov kub thiab txias los tsim ib qho khoom.
Kev siv ntawm tungsten nickel hlau alloy bar Tel: 0917-3664600
Tungsten nickel hlau rods (tseem hu ua Tungsten-raws li hnyav alloys) muaj ntau yam kev siv thoob plaws ntau yam lag luam. Qee qhov kev siv yog:
Aerospace: Tungsten-nickel-hlau rods yog siv nyob rau hauv aerospace industries rau shielding thiab ntsuas qhov ceeb thawj nyob rau hauv lub davhlau tswj chaw thiab cav.
Kev Kho Mob: Cov pas nrig no yog siv rau hauv kev kho mob cog thiab tiv thaiv hluav taws xob.
Tub rog thiab tiv thaiv: Tungsten nickel hlau rods yog siv los ua armor-choj mos txwv, missiles, thiab lwm yam riam phom.
Kev lag luam: Cov pas nrig no yog siv rau hauv kev tsim cov khoom siv X-ray, vuam electrodes, thiab cov dab dej kub.
Cov khoom ntaus pob ncaws pob: WNiFe rods yog siv los tsim cov darts thiab nuv ntses hnyav.
Automotive: W-Ni-Fe hnyav alloy tuav yog siv rau kev tsim lub cav qhov chaw thiab hauv qhov hnyav ballast rau cov tsheb sib tw.
Zuag qhia tag nrho, qhov siab ceev thiab lub zog zoo tshaj plaws ntawm tungsten nickel hlau rods ua rau lawv haum rau ntau hom kev siv uas yuav tsum muaj cov ntaub ntawv tuab.
Packing Thiab Shipping Tel: 0917-3664600

W-Ni-Fe rods yog ntau yam ntaub ntawv uas pom siv nyob rau hauv ntau yam kev siv uas yuav tsum tau muaj zog, toughness, thiab thermal conductivity, raws li zoo raws li tiv thaiv corrosion thiab hluav taws xob.
Lwm yam ntsig txogHigh-Density Tungsten Nickel Hlau Alloy (W-Ni-Fe) khoom


Cim npe nrov: tungsten nickel hlau qws w-ni-fe alloy, Tuam Tshoj, lwm tus neeg, manufacturers, hoobkas, customized, lag luam wholesale, bulk, luv nqi, kev muag, Tshuag, yuav luv nqi, ua nyob rau hauv Suav teb