Tantalum Sheet Hlau

Tantalum Sheet Hlau

Tantalum daim ntawv
R05200 Tantalum Ntawv
Tantalum Sheet & Phaj
Tau Phaj
Daim ntawv
Tantalum Ntawv ASTM B 708 UNS R05200
Tantalum alloy daim ntawv
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

 

1. Tantalum ntawv hlauyog ib daim ntawv hlau nyias ua los ntawm R05200 ntshiab tantalum thiab tantalum alloy, nws tseem hu ua Ta sheet lossis phaj, uas yog cov hlau tsis tshua muaj refractory.

2. R05200 Tantalum Sheet muaj qhov loj thiab qib

Qib: Ta1 R05200 Ta2 R05400

Txuj: ASTM B708

Purity: 99.95 feem pua ​​99.99 feem pua

Surface: sliver hlau xim

Qhov ceev: 16.5g / cm3

Melting point: 2980 degree

Tantalum Sheet metal supplier ASTM B 708 UNS R05200
buy R05200 Tantalum Sheet

3. Tshuaj muaj pes tsawg leeg

Tshuaj muaj pes tsawg leeg, Max
QibCNOHFeSiTiNiNbWMo
Ta10.0040.0050.020.0020.0050.0050.0020.0050.050.0020.002

4. Tantalum sheet hlau mechanical zog

QibXeevThickness (hli)Tensile zog (MPa)Elongation (%)
Ta1M0.1~0.5Ntau dua lossis sib npaug rau 207Ntau dua lossis sib npaug li 25
>0.5~3.0Ntau tshaj los yog sib npaug rau 30

5. Dab tsi yog daim ntawv thov ntawm R05200 Tantalum Sheet?

R05200 tantalum ntawv yog siv los ua cov khoom cua sov, cov khoom siv hluav taws xob, thiab cov khoom siv them nyiaj rau lub tshuab nqus tsev vacuum. Nws tuaj yeem siv los ua cov tshuab digesters, cua sov, cua txias, ntau yam khoom siv, thiab cov cuab yeej siv hauv kev lag luam tshuaj, nrog rau kev siv dav hauv kev lag luam aviation, aerospace, kev kho mob, thiab lwm yam.

6. Dab tsi yog tantalum sheet hlau txoj kab uas hla thiab kam rau ua?

ThicknessUa siab ntevDavW ToleranceNtevL Ua siab ntev
Qib IQib II
0.15~0.2±0.015±0.0250-300±2.0100-1000±2.0
>0.2~0.3±0.020±0.0350-300±2.0100-1000±2.0
>0.3~0.5±0.030±0.0450-300±2.0100-1000±2.0
>0.5~0.8±0.040±0.0650-200±1.050-700±2.0
>0.8~1.0±0.060±0.0850-200±1.050-700±2.0
>1.0~1.5±0.080±0.1050-200±1.050-700±2.0
>1.5~2.0±0.120±0.1450-200±1.050-700±2.0
>2.0~3.0±0.160±0.1850-200±1.050-700±2.0
>3.0~4.0±0.180±0.2050-200±1.050-700±1.0
>4.0~6.0±0.200±0.2450-200±1.050-700±1.0

7. Qhov zoo ntawmtantalum daim hlau

Tantalum hlau ntawv muaj cov tshuaj ruaj khov zoo rau cov kua qaub, alkalis, ntsev, thiab cov organic media, thib ob tsuas yog platinum thiab kub. Tantalum yuav tsis raug corroded nyob rau hauv feem ntau nruab nrab tsuas yog fluorine, hydrofluoric acid, thiab acidic tov uas muaj fluoride ions, fuming nitric acid, thiab sulfuric acid.

8. Qhov twg yuavtantalum daim hlau?

Raws li ib tug ntawm cov uas tsis tshua muaj refractory hlau tantalum daim ntawv lwm tus neeg, peb muaj ntau xyoo ntawm kev ua hlau, peb tsis muab cov neeg muas zaub nrog cov khoom zoo, tab sis kuj nrog cov qauv zoo export pob, yog tias koj xav yuav R05200 Tantalum Sheet, pls ua siab zoo tiv tauj peb ntawm sales@tmsalloy.com

R05200 Tantalum Sheet metal price


Cim npe nrov: tantalum sheet hlau, lwm tus neeg, manufacturers, hoobkas, nqe, tej, kev muag, Tshuag, yuav luv nqi